In-vitro degradation behaviour of WE54 magnesium alloy in simulated body fluid
Walter, R., and Mathan, M. Bobby (2011) In-vitro degradation behaviour of WE54 magnesium alloy in simulated body fluid. Materials Letters, 65 (4). pp. 748-750.
| PDF (Published Version) - Repository staff only - Requires a PDF viewer such as GSview, Xpdf or Adobe Acrobat Reader 448Kb |
DOI: 10.1016/j.matlet.2010.11.051
View at Publisher Website: http://dx.doi.org/10.1016/j.matlet.2010....
Abstract
Rare earths containing magnesium alloy, WE54, exhibited a marginally higher in-vitro degradation resistance than that of pure magnesium. Heat-treatment procedure had an influence on the degradation behaviour. However, comparing with AZ91 magnesium alloy the in-vitro degradation resistance of WE54 magnesium alloy was significantly lower, which suggests that the passivating capacity of rare earths is inferior to that of aluminium under in-vitro condition.
| ID Code: | 15920 |
|---|---|
| Item Type: | Article (Refereed Research - C1) |
| Keywords: | magnesium alloys; biomaterials; rare earth; corrosion |
| FoR Codes: | 09 ENGINEERING > 0903 Biomedical Engineering > 090301 Biomaterials @ 100% |
| SEO Codes: | 86 MANUFACTURING > 8611 Basic Metal Products (incl. Smelting, Rolling, Drawing and Extruding) > 861199 Basic Metal Products (incl. Smelting, Rolling, Drawing and Extruding) not elsewhere classified @ 100% |
| Deposited On: | 09 Jun 2011 10:08 |
| Last Modified: | 04 Jun 2013 01:43 |
| Downloads: | Total: 3 Last 12 Months: 0 |
| Statistics: | More Statistics |
| Citation Counts with External Providers: | Web of Science: 8 |
Repository Staff Only: item control page